White Spots

 

 

CAUSE

REMEDY
A Water mixing with the lacquer either through the "separator" or by not having the surface dry. Clean air line and "separator". Be sure surface to be finished is dry. Bleed the line at least once every shift, or every eight hours.
B Flatting paste not mixing in. Stir thoroughly and strain material if necessary.